Switch wrinkling
Reason: insufficient smoothing of the wallpaper.
Latification of seams
Reasons: curvature when gluing the canvas on inaccuity, the absence of smoothing the canvas after the wall sticker. In addition, poor smearing of the wallpaper or lack of time to absorb the glue into the canvas leads to spontaneous swelling of the canvas on the wall and layering of the seams.
Easy color change in the area of the seams, the effect of a fat spoon
Excessive smoothing of the seams with a roller, excessive pressure on the seams leads to this effect.
Bloating and swelling
They are formed with poor -quality smoothing out the canvas after the sticker on the wall, as well as when poorly smearing the wallpaper sheet or the absence of time to absorb the glue into the canvas.
Holes and gaps
Form when cutting the edges of the canvas with a blunt tool. Can occur in other areas if the wallpaper sheet is too plundered, and it is strong pressure on it.
And so to speak, the number one problem. Lack of seams when pasting wallpaper in the joint
Always pay attention to the packaging, there should be a “step” – the necessary displacement so that the seams coincide. This is especially true for embossed silkography. If the step is not specified, try to determine it yourself. Further, everything will depend on your accuracy.
If you have comments from personal experience on the issue of wallpapering, we will be happy to hear them and publish them.